All knowledge related to building construction, civil engineering, r.c.c. work, finishing work, internal plaster, external plaster, waterproofing work

Friday, April 5, 2019

TEST TO BE CARRIED OUT ON REINFORCEMENT STEEL

TEST TO BE CARRIED OUT ON REINFORCEMENT STEEL

A) Test to be carried out at site


1. Company name
Qty to be checked - 1 sample per lot per size
Frequency of checked - per lot per size
Acceptance criteria & tolerance- as per order

2. Type of steel 

Qty to be checked - 2 sample per lot per size
Frequency of checked - per lot per size
Acceptance criteria & tolerance-HYSD/ CTD/ TDR- 40/TMT/TOR- 50 As per order(Manufacturer's Test Certificate Receipt Mandatory)

3. Physical Appearance
Qty to be checked - 2 sample per lot per size
Frequency of checked - per lot per size
Acceptance criteria & tolerance-Without cracks or splits

4.Weight/meter or rolling margin
Qty to be checked - 1 sample per lot per size
Frequency of checked - per lot per size
Acceptance criteria & tolerance-8mm   = 0.395 kg/m
                                                        10mm = 0.617 kg/m
                                                         Tolerence in nominal mass + - 7%
                                                         12mm = 0.888 Kg/m
                                                          16mm = 1.58 Kg/m
                                                          Tolerence in nominal mass + - 5%
                                                          20mm = 2.47 Kg/m
                                                          25mm = 3.85 Kg/m
                                                          32mm = 6.31 Kg/m
                                                          Tolerence in nominal mass for < 16mm dia bar is + - 3%

5. Length of bar
Qty to be checked - 1 sample per lot per size
Frequency of checked - per lot per size
Acceptance criteria & tolerance- For 8 to 10mm dia  -  Length   11  to 12m
                                                                  For 16mm & above dia -  Length >12m

6. Bend test 
Qty to be checked - 1 sample per lot per size
Frequency of checked - per lot per size
Acceptance criteria & tolerance- No rupture or crack visible on the bend portion

7 Resend test
Qty to be checked - 1 sample per lot per size
Frequency of checked - per lot per size
Acceptance criteria &  tolerance- No rupture or crack visible on the bend portion

B) Test to be carried outside laboratory


1. Tensile strength
Qty to be checked - 1 sample per lot per size
Frequency of checked - each 50 ton
Acceptance criteria &  tolerance- IS: 1786 ,10% more than proof stress but not less than 485N/mm

2.Elongation
Qty to be checked - 1 sample per lot per size
Frequency of checked - each 50 ton
Acceptance criteria &  tolerance- Min. 14.5%

3. Chemical Composition
Qty to be checked - 1 sample per lot per size
Frequency of checked - each 50 ton
Acceptance criteria &  tolerance- Carbon </= 0.3%
                                                           Sulphur  </= 0.06%
                                                           Phosporous </= 0.06%
                                                           Sulphur + Phosporous  </= 0.11%
                                                           (for Fe 415)